1. The battery removed from the car accurately clear, especially its top part, check up level of electrolit and if necessary finish it to norm. |
2. The battery is charged by a current strength 5,5 And at the turned out stoppers. The gymnastics are spent prior to the beginning of plentiful gas evolution and achievement of a constancy of pressure and electrolit density in a current of 3 hours. The density of electrolit of the charged battery at 25 ° With should correspond given to the table electrolit Density at 25 ° With, g/sm3 for each climatic area. |
3. At a battery charge it is necessary to check periodically temperature of electrolit and not to suppose its increase from above 40 ° S.Esli temperature will reach 40 ° With it is necessary to reduce half зарядный a current or to interrupt gymnastics and to cool the battery to 27 ° With. |
4. The gymnastics stop, when plentiful liberation of gas in all elements of the battery will begin, and pressure and density of electrolit during last three gaugings (made through 1) will remain constants. |
5. If in the end of gymnastics the electrolit density (defined taking into account the temperature amendment) differs from specified modify it. |
6. At the raised density select a part of electrolit and add the distilled water. If density of electrolit below norm having selected it from an element, add electrolit of the raised density (1,4 g/sm3). |
7. After updating of density of electrolit continue battery gymnastics during 30 mines for electrolit hashing. |
8. Then disconnect the battery and through 30 mines measure its level in all elements. |
9. If electrolit level appears below norm add electrolit with the density corresponding to given climatic area (see tab. electrolit Density at 25 ° With, the g/sm3). |
10. If level of electrolit above norm – select its surplus a rubber pear. |